Mostrar el registro sencillo del ítem

dc.contributor.authorGarcía-Rodríguez, M.
dc.contributor.authorGonzález Souto, Lorena 
dc.contributor.authorHernández Saz, Jesús
dc.contributor.authorJuan-Juan, J.
dc.contributor.authorCalvino Gámez, José Juan 
dc.contributor.authorCazorla-Amorós, D.
dc.contributor.authorMorallón, E.
dc.contributor.otherCiencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánicaes_ES
dc.date.accessioned2026-11-18T07:44:55Z
dc.date.available2026-11-18T07:44:55Z
dc.date.issued2026
dc.identifier.issn2050-7496
dc.identifier.issn2050-7488
dc.identifier.urihttp://hdl.handle.net/10498/40692
dc.description.abstractFocused Ion Beam-Scanning Electron Microscopy (FIB-SEM) was employed to investigate the Gas Diffusion Layer (GDL), electrocatalyst, and electrolyte interface in rechargeable Zn–Air Batteries (ZABs) using Fresh and Used samples (before and after long-term electrocatalytic activity, respectively). The electrocatalyst was based on (hydro-)oxides of manganese, cobalt and lanthanum and carbon material. The results reveal a loss of material compaction in the Used sample, accompanied by the formation of pores and irregular gaps, as well as enhanced permeation of the electrocatalyst through the GDL, as evidenced in the tomogram. Interestingly, the analysis of the distribution of elements in the Used sample shows important differences, strongly dependent on their chemical properties in the electrolyte used. Mn and Co, the more electroactive elements for the oxygen-involved reactions, remain in proximity to the electrolyte interface, while La forms a preferential region more distant from and parallel to the electrolyte. XPS results indicate that the formation of this region is associated with the generation of lanthanum acetate species, which are responsible for the decrease in conductivity of the Used sample, as demonstrated by electrochemical impedance spectroscopy experiments, in addition to impairing O2 diffusion along the GDL. Furthermore, DFT calculations support that the formation of lanthanum acetate species from the metal (hydro)oxides is energetically favorable in the presence of zinc acetate electrolyte in ZABs.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.publisherRoyal Society of Chemistryes_ES
dc.rightsAtribución-NoComercial 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by-nc/4.0/es_ES
dc.sourceJournal of Materials Chemistry A - 2026, Vol. 14 n.16 pp. 9277-9290es_ES
dc.subjectDegradation mechanismes_ES
dc.subjectMetal analysises_ES
dc.subjectElectrocatalytic activityes_ES
dc.subjectAcetate specieses_ES
dc.titleUnraveling the interfacial degradation mechanism of a metal oxide electrocatalyst/gas diffusion layer in Zn–air batteries through FIB-SEM analysises_ES
dc.typejournal articlees_ES
dc.rights.accessRightsopen accesses_ES
dc.identifier.doi10.1039/D5TA10107G
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI/2021-2023 Plan Estatal de Investigación Científica y Técnica y de Innovación/PID2022-137566OB-I00/ES/MATERIALES 2D PARA APLICACIONES ELECTROQUIMICAS EN EL ALMACENAMIENTO Y CONVERSION DE ENERGIA/es_ES
dc.type.hasVersionVoRes_ES


Ficheros en el ítem

Este ítem aparece en la(s) siguiente(s) colección(ones)

Mostrar el registro sencillo del ítem

Atribución-NoComercial 4.0 Internacional
Esta obra está bajo una Licencia Creative Commons Atribución-NoComercial 4.0 Internacional