Show simple item record

dc.contributor.authorRuiz Jorge, Francisco
dc.contributor.authorBenítez, Almudena
dc.contributor.authorGarcía Jarana, María Belén 
dc.contributor.authorSánchez Oneto, Jezabel 
dc.contributor.authorPortela Miguélez, Juan Ramón 
dc.contributor.authorMartínez de la Ossa Fernández, Enrique José 
dc.contributor.otherIngeniería Química y Tecnología de Alimentoses_ES
dc.date.accessioned2021-12-09T12:43:57Z
dc.date.available2021-12-09T12:43:57Z
dc.date.issued2021-09
dc.identifier.issn2079-4991
dc.identifier.urihttp://hdl.handle.net/10498/25836
dc.description.abstractLithium-ion batteries (LIBs) have gained much interest in recent years because of the increasing energy demand and the relentless progression of climate change. About 30% of the manufacturing cost for LIBs is spent on cathode materials, and its level of development is lower than the negative electrode, separator diaphragm and electrolyte, therefore becoming the "controlling step". Numerous cathodic materials have been employed, LiFePO4 being the most relevant one mainly because of its excellent performance, as well as its rated capacity (170 mA center dot h center dot g(-1)) and practical operating voltage (3.5 V vs. Li+/Li). Nevertheless, producing micro and nanoparticles with high purity levels, avoiding the formation of iron oxides, and reducing the operating cost are still some of the aspects still to be improved. In this work, we have applied two heating rates (slow and fast) to the same hydrothermal synthesis process with the main objective of obtaining, without any reducing agents, the purest possible LiFePO4 in the shortest time and with the lowest proportion of magnetite impurities. The reagents initially used were: FeSO4, H3PO4, and LiOH, and a crucial phenomenon has been observed in the temperature range between 130 and 150 degrees C, being verified with various techniques such as XRD and SEM.es_ES
dc.description.sponsorshipA. Benitez thanks the financial support from the European Social Fund and Junta de Andalucia. Finally, the authors wish to acknowledge the technical staff from the University Institute of Nanochemistry (IUNAN) of the University of Cordoba. This research received no external funding.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.publisherMDPIes_ES
dc.rightsAtribución 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/*
dc.sourceNanomaterials 2021, 11(9), 2412es_ES
dc.subjectlithium iron phosphatees_ES
dc.subjecthydrothermal synthesises_ES
dc.subjectheating ratees_ES
dc.subjectmorphologyes_ES
dc.subjectcrystallinity and purityes_ES
dc.titleEffect of the Heating Rate to Prevent the Generation of Iron Oxides during the Hydrothermal Synthesis of LiFePO4es_ES
dc.typejournal articlees_ES
dc.rights.accessRightsopen accesses_ES
dc.identifier.doi10.3390/nano11092412


Files in this item