| dc.contributor.author | Morales Sánchez, Francisco Miguel | |
| dc.contributor.author | Escanciano, Marta | |
| dc.contributor.author | Yeste Siguenza, María del Pilar | |
| dc.contributor.author | Santos Izquierdo-Bueno, Antonio Jesús | |
| dc.contributor.other | Ciencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánica | es_ES |
| dc.date.accessioned | 2022-07-01T09:50:20Z | |
| dc.date.available | 2022-07-01T09:50:20Z | |
| dc.date.issued | 2022-05 | |
| dc.identifier.issn | 2079-4991 | |
| dc.identifier.uri | http://hdl.handle.net/10498/27094 | |
| dc.description.abstract | A mechanistic study was carried out on the optimal methods of fabrication of products containing higher loads of thermochromic VO2(M1) fabricated by thermal treatments of V nanoparticles in air, that, once achieved, are more stable than other commercial products upon natural aging or reiterated reheating. At the best temperatures for single runs, 55% of VO2 can be attained by the reactions of a limited number of the species initially formed in a process, that, if not stopped, can degrade the product by solid state reactions of oxidations and reductions without O-2 consumption. This fact supports the use of two-step treatments at lower temperatures and faster cooling rates that reach 65% of VO2; such reactions should, ideally, take place in the 550-625 degrees C temperature range. The impregnation of V with a tungstate salt is an ideal and simple doping platform that can decrease the energy of activation of the 2-cycle process, allowing higher yields and enthalpies of transformation (71% of VO2, 26 J/g) than undoped counterparts or trademarks. A good balance is reached for 1% at. of W, with a reduction in T-c of 20 degrees C not significantly resenting the enthalpy of the reversible metal-to-insulator transition. For higher W amounts, the appearance of tetragonal VO2, and W alloyed V3O7 and V2O5, decrease the fractions of increasingly and effectively doped M1-VO2 achieved till 2% of W, a concentration for which T-c attains the stimulating values of 35 degrees C on heating and 25 degrees C on cooling. | es_ES |
| dc.format | application/pdf | es_ES |
| dc.language.iso | eng | es_ES |
| dc.publisher | MDPI | es_ES |
| dc.rights | Atribución 4.0 Internacional | * |
| dc.rights.uri | http://creativecommons.org/licenses/by/4.0/ | * |
| dc.source | Nanomaterials, Vol. 12, Núm. 9 | es_ES |
| dc.subject | vanadium oxidation | es_ES |
| dc.subject | vanadium dioxide synthesis | es_ES |
| dc.subject | vanadium dioxide doping | es_ES |
| dc.subject | X-ray diffraction | es_ES |
| dc.subject | differential scanning calorimetry | es_ES |
| dc.title | Reactivity of Vanadium Nanoparticles with Oxygen and Tungsten | es_ES |