Show simple item record

dc.contributor.authorMary Joy, Rani
dc.contributor.authorPobedinskas, Paulius
dc.contributor.authorBaule, N
dc.contributor.authorBai, S
dc.contributor.authorJannis, D
dc.contributor.authorGaquelin, N
dc.contributor.authorPinault-Thaury, Marie-Amandine
dc.contributor.authorJomard, F
dc.contributor.authorJothiramalingam Sankaran, Kamatchi
dc.contributor.authorRouzbahani, Rozita
dc.contributor.authorLloret Vieira, Fernando Manuel 
dc.contributor.authorDesta, Derese
dc.contributor.authorD´haen, J
dc.contributor.authorVerbeeck, J
dc.contributor.authorBecker, MF
dc.contributor.authorHaenen, Ken
dc.contributor.otherFísica Aplicadaes_ES
dc.date.accessioned2024-02-02T16:34:00Z
dc.date.available2024-02-02T16:34:00Z
dc.date.issued2024
dc.identifier.issn1359-6454
dc.identifier.urihttp://hdl.handle.net/10498/30528
dc.description.abstractThis study reports the impact of film microstructure and composition on the Young's modulus and residual stress in nanocrystalline diamond (NCD) thin films (≈250nm thick) grown on silicon substrates using a linear antenna microwave plasma-enhanced chemical vapor deposition (CVD) system. Combining laser acoustic wave spectroscopy to determine the elastic properties with simple wafer curvature measurements, a straightforward method to determine the intrinsic stress in NCD films is presented. Two deposition parameters are varied: (1) the substrate temperature from 400 °C to 900 °C, and (2) the [P]/[C] ratio from 0 ppm to 8090 ppm in the H2/CH4/CO2/PH3 diamond CVD plasma. The introduction of PH3 induces a transition in the morphology of the diamond film, shifting from NCD with larger grains to ultra-NCD with a smaller grain size, concurrently resulting in a decrease in Young's modulus. Results show that the highest Young's modulus of (1130±50) GPa for the undoped NCD deposited at 800 °C is comparable to single crystal diamond, indicating that NCD with excellent mechanical properties is achievable with our process for thin diamond films. Based on the film stress results, we propose the origins of tensile intrinsic stress in the diamond films. In NCD, the tensile intrinsic stress is attributed to larger grain size, while in ultra-NCD films the tensile intrinsic stress is due to grain boundaries and impurities.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.sourceActa Materialia, Vol. 264es_ES
dc.subjectLinear antennaes_ES
dc.subjectCVD reactores_ES
dc.subjectNanocrystalline diamondes_ES
dc.subjectYoung’s moduluses_ES
dc.subjectResidual stresses_ES
dc.titleThe effect of microstructure and film composition on the mechanical properties of linear antenna CVD diamond thin filmses_ES
dc.typejournal articlees_ES
dc.rights.accessRightsclosed accesses_ES
dc.identifier.doi10.1016/J.ACTAMAT.2023.119548
dc.type.hasVersionVoRes_ES


Files in this item

This item appears in the following Collection(s)

Show simple item record