Show simple item record

dc.contributor.authorUtrilla, Antonio D.
dc.contributor.authorGrossi, Davide F.
dc.contributor.authorFernández de los Reyes, Daniel 
dc.contributor.authorGonzalo, Alicia
dc.contributor.authorBraza Blanco, María Verónica 
dc.contributor.authorBen Fernández, Teresa 
dc.contributor.authorGonzález Robledo, David 
dc.contributor.authorGuzman, Alvaro
dc.contributor.authorHierro, Adrian
dc.contributor.authorKoenraad, Paul M.
dc.contributor.authorUlloa, Jose M.
dc.contributor.otherCiencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánicaes_ES
dc.date.accessioned2024-02-08T10:32:19Z
dc.date.available2024-02-08T10:32:19Z
dc.date.issued2018
dc.identifier.issn0169-4332
dc.identifier.urihttp://hdl.handle.net/10498/30827
dc.description.abstractThe practical realization of epitaxial quantum dot (QD) nanocrystals led before long to impressive experimental advances in optoelectronic devices, as well as to the emergence of new technological fields. However, the necessary capping process is well-known to hinder a precise control of the QD morphology and therefore of the possible electronic structure required for certain applications. A straightforward approach is shown to tune the structural and optical properties of InAs/GaAs QDs without the need for any capping material different from GaAs or annealing process. The mere adjust of the capping rate allows controlling kinetically the QD dissolution process induced by the surface In-Ga intermixing taking place during overgrowth, determining the final metastable structure. While low capping rates make QDs evolve into more thermodynamically favorable quantum ring structures, increasing capping rates help preserve the QD height and shape, simultaneously improving the luminescence properties. Indeed, a linear relationship between capping rate and QD height is found, resulting in a complete preservation of the original QD geometry for rates above ∼2.0 ML s −1 . In addition, the inhibition of In diffusion from the QDs top to the areas in between them yields thinner WLs, what could improve the performance of several QD-based optoelectronic devices.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.publisherElsevieres_ES
dc.sourceApplied Surface Science - 2018, Vol. 444, pp. 260 - 26630es_ES
dc.subjectCapping rate; Dissolution process; Molecular beam epitaxy; Quantum dot; Quantum ring; Wetting layeres_ES
dc.titleSize and shape tunability of self-assembled InAs/GaAs nanostructures through the capping ratees_ES
dc.typejournal articlees_ES
dc.rights.accessRightsclosed accesses_ES
dc.identifier.doi10.1016/j.apsusc.2018.03.098
dc.relation.projectIDinfo:eu-repo/grantAgreement/MINECO//MAT2013-47102-C2-2-R/ES/ALEACIONES EMERGENTES DE NITRUROS DILUIDOS III-V Y NANOESTRUCTURAS RELACIONADAS PARA APLICACIONES FOTOVOLTAICAS Y DE FOTODETECCION DE ALTA EFICIENCIA/ es_ES
dc.relation.projectIDMAT2016-77491-C2-1-Res_ES
dc.type.hasVersionVoRes_ES