Show simple item record

dc.contributor.authorAmaya Dolores, Beatriz 
dc.contributor.authorRuiz Flores, Andrés
dc.contributor.authorNúñez Galindo, Andrés
dc.contributor.authorCalvino Gámez, José Juan 
dc.contributor.authorAlmagro Bello, Juan F.
dc.contributor.authorLajaunie, Luc Cyrille Jacques 
dc.contributor.otherCiencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánicaes_ES
dc.date.accessioned2024-04-30T10:27:57Z
dc.date.available2024-04-30T10:27:57Z
dc.date.issued2023
dc.identifier.issn1996-1944
dc.identifier.urihttp://hdl.handle.net/10498/32043
dc.description.abstractThe “gold dust defect” (GDD) appears at the surface of ferritic stainless steels (FSS) and degrades their appearance. Previous research showed that this defect might be related to intergranular corrosion and that the addition of aluminium improves surface quality. However, the nature and origin of this defect are not properly understood yet. In this study, we performed detailed electron backscatter diffraction analyses and advanced monochromated electron energy-loss spectroscopy experiments combined with machine-learning analyses in order to extract a wealth of information on the GDD. Our results show that the GDD leads to strong textural, chemical, and microstructural heterogeneities. In particular, the surface of affected samples presents an -fibre texture which is characteristic of poorly recrystallised FSS. It is associated with a specific microstructure in which elongated grains are separated from the matrix by cracks. The edges of the cracks are rich in chromium oxides and MnCr2O4 spinel. In addition, the surface of the affected samples presents a heterogeneous passive layer, in contrast with the surface of unaffected samples, which shows a thicker and continuous passive layer. The quality of the passive layer is improved with the addition of aluminium, explaining the better resistance to the GDD.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.publisherMDPIes_ES
dc.rightsAttribution-NonCommercial-NoDerivatives 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.sourceMaterials - 2023, Vol. 16 n.5 pp. 1-14es_ES
dc.subjectferritic stainless steeles_ES
dc.subjectAISI 430es_ES
dc.subjectgrains texturees_ES
dc.subjectelectron backscatter diffraction (EBSD)es_ES
dc.subjectmicrostructurees_ES
dc.subjecttransmission electron microscopy (TEM)es_ES
dc.subjectmonochromated electron energy-loss spectroscopy (EELS)es_ES
dc.subjectoxidations stateses_ES
dc.subjectmachine learninges_ES
dc.subjectk-means clusteringes_ES
dc.titleTextural, Microstructural and Chemical Characterization of Ferritic Stainless Steel Affected by the Gold Dust Defectes_ES
dc.typejournal articlees_ES
dc.rights.accessRightsopen accesses_ES
dc.identifier.doi10.3390/MA16051825
dc.relation.projectIDinfo:eu-repo/grantAgreement/Junta de Andalucía//FEDER-UCA18-107490es_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/EC/H2020/823717/EU es_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI/Plan Estatal de Investigación Científica y Técnica y de Innovación 2017-2020/PID2019-107578GA-I00/ES/COMBINACION DE PLASMONICA Y CATALISIS PARA EL DESARROLLO DE NANOESTRUCTURAS BASADAS EN MOS2 PARA APLICACIONES DE ENERGIA LIMPIA/ es_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI//RYC2021-033764-Ies_ES
dc.type.hasVersionVoRes_ES


Files in this item

This item appears in the following Collection(s)

Show simple item record

Attribution-NonCommercial-NoDerivatives 4.0 Internacional
This work is under a Creative Commons License Attribution-NonCommercial-NoDerivatives 4.0 Internacional