Show simple item record

dc.contributor.authorAmaya Dolores, Beatriz 
dc.contributor.authorNúñez Galindo, Andrés
dc.contributor.authorCalvino Gámez, José Juan 
dc.contributor.authorAlmagro, Juan Francisco
dc.contributor.authorLajaunie, Luc Cyrille Jacques 
dc.contributor.otherCiencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánicaes_ES
dc.date.accessioned2024-06-04T13:05:19Z
dc.date.available2024-06-04T13:05:19Z
dc.date.issued2023
dc.identifier.issn2238-7854
dc.identifier.urihttp://hdl.handle.net/10498/32486
dc.description.abstractThe “Gold Dust Defect” that sometimes appears on the surface of the AISI 430 ferritic stainless steel has been related to an improper recrystallization of the material. Hot-rolling, a decisive step in the production process, seems the step where this defect is induced and temperature during this treatment plays a key role. To trace back the origin of this defect, the microstructural evolution of a sample of an AISI 430 was monitored at the different stages in the production process of the steel. In particular, a detailed study combining electron backscatter diffraction with other techniques, such as optical microscopy and scanning electron microscopy has been performed. The whole set of results evidences that after hot-rolling and subsequent annealing, the material contains a large amount of martensite in the center of the cross-section due to a fast cooling of the austenite originated during rolling. In addition, the surface shows a top-layer made up by unrecrystallized subgrains separated from the matrix by an accumulation of chromium carbides. After pickling, the top-layer of subgrains semi-detaches from the surface forming flakes which cannot recrystallize. Most of these flakes do not peel off during the subsequent stages but survive until the end of the production process, forming Gold Dust Defect flakes.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.publisherElsevieres_ES
dc.rightsAtribución 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/*
dc.sourceJournal of Materials Research and Technology, Vol. 25, 2023, pp. 7444-7453es_ES
dc.subjectEBSDes_ES
dc.subjectFerritic stainless steeles_ES
dc.subjectGold Dust Defectes_ES
dc.subjectHot-rollinges_ES
dc.subjectRecrystallizationes_ES
dc.subjectSubgrainses_ES
dc.titleOn the likely origin of the Gold Dust Defect in the production line of industrial ferritic stainless steeles_ES
dc.typejournal articlees_ES
dc.rights.accessRightsopen accesses_ES
dc.identifier.doi10.1016/J.JMRT.2023.07.127
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI/Plan Estatal de Investigación Científica y Técnica y de Innovación 2017-2020/PID2019-107578GA-I00/ES/COMBINACION DE PLASMONICA Y CATALISIS PARA EL DESARROLLO DE NANOESTRUCTURAS BASADAS EN MOS2 PARA APLICACIONES DE ENERGIA LIMPIA/ es_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/Junta de Andalucía//FEDER-UCA18-107490es_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI//RYC2021-033764-Ies_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/EC/H2020/823717/EU es_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI/Plan Estatal de Investigación Científica y Técnica y de Innovación 2021-2023/CPP2021-008986/ES/HIDRÓGENO: ENVASES A PRESIÓN EN ACERO INOXIDABLEes_ES
dc.type.hasVersionVoRes_ES


Files in this item

This item appears in the following Collection(s)

Show simple item record

Atribución 4.0 Internacional
This work is under a Creative Commons License Atribución 4.0 Internacional