Show simple item record

dc.contributor.authorDupré, Nicolas
dc.contributor.authorWang, Zhongli
dc.contributor.authorLajaunie, Luc Cyrille Jacques 
dc.contributor.authorMoreau, Philippe
dc.contributor.authorMartin, Jean-Frederic
dc.contributor.authorBoutafa, Laura
dc.contributor.authorPatoux, Sebastien
dc.contributor.authorGuyomard, Dominique
dc.contributor.otherCiencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánicaes_ES
dc.date.accessioned2025-01-21T17:14:42Z
dc.date.available2025-01-21T17:14:42Z
dc.date.issued2012
dc.identifier.issn0378-7753
dc.identifier.urihttp://hdl.handle.net/10498/34623
dc.description.abstractInvestigation of electrode/electrolyte interface of 5V spinel material LiNi0.4Mn1.6O4 was carried out in the presence of glutaric anhydride additive, using combined magic angle spinning NMR spectroscopy and electron energy-loss spectroscopy. After exposure to LiPF6 in EC/DMC liquid electrolyte, oxidation state of +III or lower has been evidenced by EELS for Mn ions, indicating that the presence of glutaric anhydride additive in the electrolyte, not only modifies the interphase, but does not prevent chemical reactions with the active material. Further investigation of the influence of the additive upon storage and cycling was performed using combined 7Li and 19F MAS NMR. The native interphase formed by simple contact of the active material with the electrolyte is partially destroyed at high potential but the new appearing interphase is overall increasing upon cycling, independently from the presence of glutaric anhydride. The use of glutaric anhydride is nevertheless beneficial as it clearly restrains the formation of lithiated interphasial species and alters the interphase composition since the formation of fluorophosphates is promoted, lowering the relative amount of resistive LiF. Although resistive LiF can be formed in significant amount, it is removed by the DMC rinsing while fluorophosphates display a stronger adherence to the active material.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.rightsAttribution-NonCommercial-NoDerivatives 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.sourceJournal of Power Sources 215:170-178 2012es_ES
dc.titleEffect of glutaric anhydride additive on the LiNi0.4Mn1.6O4 electrode/electrolyte interface evolution: A MAS NMR and TEM/EELS studyes_ES
dc.typejournal articlees_ES
dc.rights.accessRightsopen accesses_ES
dc.identifier.doi10.1016/j.jpowsour.2012.05.027
dc.type.hasVersionSMURes_ES


Files in this item

This item appears in the following Collection(s)

Show simple item record

Attribution-NonCommercial-NoDerivatives 4.0 Internacional
This work is under a Creative Commons License Attribution-NonCommercial-NoDerivatives 4.0 Internacional