Show simple item record

dc.contributor.authorValendolf Nunes, Jackeline 
dc.contributor.authorLeinen, D.
dc.contributor.authorAlba Muñoz, Gonzalo 
dc.contributor.authorLloret Vieira, Fernando Manuel 
dc.contributor.authorPiñero Charlo, José Carlos 
dc.contributor.authorSuzuki, Mariko 
dc.contributor.authorAraújo Gay, Daniel 
dc.contributor.otherCiencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánicaes_ES
dc.contributor.otherDidácticaes_ES
dc.contributor.otherFísica Aplicadaes_ES
dc.date.accessioned2025-02-21T10:27:16Z
dc.date.available2025-02-21T10:27:16Z
dc.date.issued2024-08-31
dc.identifier.issn0169-4332
dc.identifier.urihttp://hdl.handle.net/10498/35556
dc.description.abstractAmong diamond-based devices, the Schottky barrier diode (SBD) shows significant promise, achieving high breakdown voltages (9.5 MV⋅cm ) and reduced serial resistance (1 Ω) through structural advancements. The performance of SBDs depends on the interface between the Schottky contact, surface termination, and diamond. Studies have highlighted the impact of interface configuration on Schottky barrier height (SBH), particularly for hydrogen (H) and oxygen (O)-terminated diamonds. H-terminated surfaces exhibit negative electron affinity (NEA), whereas O-terminated surfaces show positive electron affinity (PEA). This surface behaviour has a strong impact on electron affinity, surface conductivity, work function, and the SBH which are critical for device performance. To know more about the metal-surface-diamond interface, tungsten (W) and platinum (Pt) deposited by electron beam-induced deposition (EBID), in a FIB dual beam, were employed as Schottky contacts on H and O-terminated diamond. The resulting structure has a pseudo vertical configuration with a back ohmic contact on a p ++ boron-doped layer. The current–voltage (I-V) and X-ray photoelectron spectroscopy (XPS) measurements resulted in a SBH of 1.69 eV for W and 1.76 eV for Pt, with an ideal factor (n) of 1.22 and 1.18, respectively. These n values demonstrated a chemical reactivity between metal-surface-diamond. Finally, a combination of two techniques for the SBH estimation is discussed.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.publisherElsevieres_ES
dc.rightsAttribution-NonCommercial-NoDerivatives 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.sourceApplied Surface Science 674 (2024) 160909es_ES
dc.subjectDiamondes_ES
dc.subjectEBIDes_ES
dc.subjectSchottky barrier heightes_ES
dc.subjectSurface treatmentes_ES
dc.subjectXPSes_ES
dc.titleFIB in-situ fabrication of pseudo vertical diamond Schottky diode: H-terminated ohmic contact and O-terminated Schottky barrieres_ES
dc.typejournal articlees_ES
dc.rights.accessRightsopen accesses_ES
dc.identifier.doi10.1016/j.apsusc.2024.160909
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI/Plan Estatal de Investigación Científica y Técnica y de Innovación 2017-2020/PID2020-117201RB-C21/ES/NUEVOS CONFIGURACIONES DE PUERTAS PARA MISFETS DE DIAMANTE CON CANAL OPTO-ACTIVADO :CRECIMIENTO Y CARACTERIZACION/ es_ES
dc.relation.projectIDinfo:eu-repo/grantAgreement/AEI//PDC2023-145907-I00es_ES
dc.type.hasVersionVoRes_ES


Files in this item

This item appears in the following Collection(s)

Show simple item record

Attribution-NonCommercial-NoDerivatives 4.0 Internacional
This work is under a Creative Commons License Attribution-NonCommercial-NoDerivatives 4.0 Internacional