SEM and EDS Characterisation of Layering TiOx Growth onto the Cutting Tool Surface in Hard Drilling Processes of Ti-Al-V Alloys

Thumbnail
Identificadores

URI: http://hdl.handle.net/10498/35760

DOI: 10.1155/2011/414868

ISSN: 1687-8434

ISSN: 1687-8442

Files
Advances in Materials Science and Engineering - 2011 - Álvarez - SEM and EDS Characterisation of Layering TiOx Growth onto.pdf (9.437Mb)
Statistics
View statistics
Metrics and citations
 
Share
Export
Export reference to MendeleyRefworksEndNoteBibTexRIS
Metadata
Show full item record
Author/s
Álvarez Alcón, MiguelAuthority UCA; Salguero Gómez, JorgeAuthority UCA; Sánchez, J.A.; Huerta Gómez de Merodio, MilagrosAuthority UCA; Marcos Bárcena, Mariano
Date
2011-09-21
Department
Ingeniería Mecánica y Diseño Industrial
Source
Advances in Materials Science and Engineering, Vol. 2011, 2011
Abstract
Scanning electron microscopy (SEM) has been used to identify and analyse the secondary adhesion effect precursors formed during the dry drilling processes of Ti-6Al-4V alloy over the rake face and flute of the drilling tools. Subsequent analysis with energy dispersive spectroscopy (EDS) was enabled to distinguish its compositional characteristics. Thus, according to the EDS obtained data, a stratified multi built-up layer (MBUL) composed by TiOx is formed over the rake face of the tool. Furthermore, this multi-layer adhered allows initially the built-up edge (BUE) development close to the edge of the tool by a mechanical adhesion mechanism. In a second step, it is responsible for the formation of a thicker secondary BUL which avoids the chip flow, and it provokes the tool collapse. These mechanisms are different from those observed in the dry machining of other alloys such as steels, nickel-based alloys, or aluminium alloys.
Collections
  • Artículos Científicos [11954]
  • Articulos Científicos Ing. Mec. [324]
Attribution-NonCommercial-NoDerivatives 4.0 Internacional
This work is under a Creative Commons License Attribution-NonCommercial-NoDerivatives 4.0 Internacional

Browse

All of RODINCommunities and CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

My Account

LoginRegister

Statistics

View Usage Statistics

Información adicional

AboutDeposit in RODINPoliciesGuidelinesRightsLinksStatisticsNewsFrequently Asked Questions

RODIN is available through

OpenAIREOAIsterRecolectaHispanaEuropeanaBaseDARTOATDGoogle Academic

Related links

Sherpa/RomeoDulcineaROAROpenDOARCreative CommonsORCID

RODIN está gestionado por el Área de Biblioteca, Archivo y Publicaciones de la Universidad de Cádiz

Contact informationSuggestionsUser Support