Show simple item record

dc.contributor.authorMallik, Awadesh Kumar
dc.contributor.authorJothiramalingam Sankaran, Kamatchi
dc.contributor.authorDesta, Derese
dc.contributor.authorPobedinskas, Paulius
dc.contributor.authorMary Joy, Rani
dc.contributor.authorRouzbahani, Rozita
dc.contributor.authorLloret Vieira, Fernando Manuel 
dc.contributor.authorBoyen, Hans-Gerd
dc.contributor.authorHaenen, Ken
dc.contributor.otherFísica Aplicadaes_ES
dc.date.accessioned2025-09-10T16:23:29Z
dc.date.available2025-09-10T16:23:29Z
dc.date.issued2024
dc.identifier.issn2296-598X
dc.identifier.urihttp://hdl.handle.net/10498/37161
dc.description.abstractIntegrating chemical vapour deposition (CVD) diamond with GaN material for effective thermal management of the power electronic devices is critical. However, there are issues with CVD processing, like GaN substrate etching under normal CVD diamond growth conditions, which nowadays, is overcome by inserting an intermediate silicon nitride layer of very low thermal conductivity. Unfortunately, such a buffer layer is detrimental to proper heat dissipation. So, the direct growth of diamonds onto GaN substrates is still a relevant research topic. Here, we have used an innovative low-temperature growth process by linear antenna microwave plasma enhanced CVD to overcome such a problem. Other than the normal hydrogen gas CVD recipe, PH3 gas diluted with hydrogen (1,000 ppm in H2) was added as a doping gas precursor, to dope the diamond lattice with phosphorous atoms, by varying the substrate temperature from 400oC to 900oC. PH3 addition in the precursor gas recipe was found to etch the GaN substrate substantially. The phosphorous atom was found to be present on the surface of the diamond film from their corresponding X-ray photoelectron spectroscopy signal. Raman spectroscopy and scanning electron microscopy images do not reveal GaN substrate damage when pure hydrogen gas was used as a precursor without PH3 addition. However, there is a relative competition between the GaN substrate decomposition and CVD diamond growth rates when diluted PH3 gas was used in the precursor gas recipe. At a lower substrate temperature of 400oC, GaN etching was prevalent, but with a gradual increase in substrate temperature to 900ºC, diamond lateral growth was promoted inside the linear antenna CVD reactor, which partially protected the underneath GaN/sapphire heterostructures from decomposition under harsh plasma CVD conditions.es_ES
dc.formatapplication/pdfes_ES
dc.language.isoenges_ES
dc.publisherFrontierses_ES
dc.rightsAtribución 4.0 Internacional*
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/*
dc.sourceFrontiers in Energy Research, Vol. 12, 2024es_ES
dc.subjectdiamondes_ES
dc.subjectGaNes_ES
dc.subjectchemical vapor depositiones_ES
dc.subjectphosphinees_ES
dc.subjecthydrogenes_ES
dc.subjectetchinges_ES
dc.titleLACVD growth of diamond on gallium nitride substrates with PH3 in recipees_ES
dc.typejournal articlees_ES
dc.rights.accessRightsopen accesses_ES
dc.identifier.doi10.3389/FENRG.2024.1413495
dc.type.hasVersionVoRes_ES


Files in this item

This item appears in the following Collection(s)

Show simple item record

Atribución 4.0 Internacional
This work is under a Creative Commons License Atribución 4.0 Internacional