Multiscale Analysis of the Gold Dust Defect in AISI 430 Industrial Stainless Steels: Influence of the Aluminum Content

Thumbnail
Identificadores

URI: http://hdl.handle.net/10498/27611

DOI: 10.1007/s11837-022-05478-8

ISSN: 1543-1851

Ficheros
APC_2022_123.pdf (5.254Mb)
Estadísticas
Ver estadísticas
Métricas y Citas
 
Compartir
Exportar a
Exportar a MendeleyRefworksEndNoteBibTexRIS
Metadatos
Mostrar el registro completo del ítem
Autor/es
Amaya Dolores, BeatrizAutoridad UCA; Letofsky-Papst, Ilse; Domínguez de la Vega, ManuelAutoridad UCA; Núñez Galindo, Andrés; Calvino Gámez, José JuanAutoridad UCA; Almagro Bello, Juan F.; Lajaunie, Luc Cyrille JacquesAutoridad UCA
Fecha
2022-11
Departamento/s
Ciencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánica; Física de la Materia Condensada
Fuente
JOM, Vol. 74, Núm. 11, pp. 4059-4068
Resumen
The "Gold Dust Defect" affects the surface quality of AISI 430 ferritic stainless steels. However, there is a very limited number of studies focusing on it. To better understand its nature, we have combined several techniques, such as x-ray photoelectron spectroscopy, atomic force microscopy, and transmission electron microscopy, in order to extract a maximum of structural and compositional information. Our results show that the surface quality, microstructure, and chemistry of the samples are strongly affected by the aluminum content, the severity of the defect being the highest at the lowest Al concentration. Not only is the concentration of the defects at the surface strongly reduced when increasing the Al. at.% but the depth of the cavities is also reduced by a factor of 3 when the Al content is increased from 0.09 at.% to 0.59 at.%. Our results provide new information on the nature of this defect, and show that an increase of the aluminum content allows the Cr concentration to be maintained in the range of values required to maintain the passivity of the steel, thus improving the surface quality.
Colecciones
  • Artículos Científicos [12023]
  • Articulos Científicos CC. Mat. [583]
  • Articulos Científicos Fis. Mat. Cond. [129]
  • Artículos Científicos IMEYMAT [578]
  • OpenAIRE [58]
Atribución 4.0 Internacional
Esta obra está bajo una Licencia Creative Commons Atribución 4.0 Internacional

Listar

Todo RODINComunidades y ColeccionesPor fecha de publicaciónAutoresTítulosMateriasEsta colecciónPor fecha de publicaciónAutoresTítulosMaterias

Mi cuenta

AccederRegistro

Estadísticas

Ver Estadísticas de uso

Información adicional

Acerca de...Deposita en RODINPolíticasNormativasDerechos de autorEnlaces de interésEstadísticasNovedadesPreguntas frecuentes

RODIN está accesible a través de

OpenAIREOAIsterRecolectaHispanaEuropeanaBaseDARTOATDGoogle Académico

Enlaces de interés

Sherpa/RomeoDulcineaROAROpenDOARCreative CommonsORCID

RODIN está gestionado por el Área de Biblioteca, Archivo y Publicaciones de la Universidad de Cádiz

ContactoSugerenciasAtención al Usuario