Improved Design of Electroforming Equipment for the Manufacture of Sinker Electrical Discharge Machining Electrodes with Microtextured Surfaces

Thumbnail
Identificadores

URI: http://hdl.handle.net/10498/36738

DOI: 10.3390/ma18091972

ISSN: 1996-1944

Ficheros
046. 2025. MATERIALS (JCR Q2-T1). Improved Design of Electroforming ...pdf (14.68Mb)
Estadísticas
Ver estadísticas
Métricas y Citas
 
Compartir
Exportar a
Exportar a MendeleyRefworksEndNoteBibTexRIS
Metadatos
Mostrar el registro completo del ítem
Autor/es
Hernández Pérez, Mariana; Hernández Castellano, Pedro Manuel; Salguero Gómez, JorgeAutoridad UCA; Sánchez Morales, Carlos Jesús
Fecha
2025
Departamento/s
Ingeniería Mecánica y Diseño Industrial
Fuente
Materiales -2025, Vol.18 n.9
Resumen
The development of microtextures has had a transformative impact on surface design in engineering, leading to substantial advancements in the performance, efficiency, and functionality of components and tools. This study presents an innovative methodology for fabricating SEDM electrodes. The methodology combines additive manufacturing by mask stereolithography with an optimized electroforming process to obtain high-precision copper shells. A key aspect of the study involved redesigning the electroforming equipment, enabling the independent examination of critical variables such as anode–cathode distance and electrolyte recirculation. This approach allowed precise analysis of their impact on metal deposition. This redesign enabled the assessment of the impact of electrolyte recirculation on the quality of the shells obtained. The findings indicate that continuous recirculation at 60% power effectively reduced thickness deviation by up to 32.5% compared to the worst-case scenario, achieving average thicknesses within the functional zone of approximately 110 μm. In contrast, the absence of flow or excessive turbulence did not generate defects such as unfilled zones or non-uniform thicknesses. The shells obtained were validated as functional tools in SEDM, demonstrating their viability for the generation of textures with high geometric fidelity. This approach optimizes the manufacturing of textured electrodes and opens new opportunities for their application in advanced industrial processes, providing a more efficient and sustainable alternative to conventional methods.
Materias
micro-electroforming; microtexturing surfaces; SEDM; stereolithography by mask (MSLA)
Colecciones
  • Artículos Científicos [11977]
  • Articulos Científicos Ing. Mec. [325]
Attribution 4.0 Internacional
Esta obra está bajo una Licencia Creative Commons Attribution 4.0 Internacional

Listar

Todo RODINComunidades y ColeccionesPor fecha de publicaciónAutoresTítulosMateriasEsta colecciónPor fecha de publicaciónAutoresTítulosMaterias

Mi cuenta

AccederRegistro

Estadísticas

Ver Estadísticas de uso

Información adicional

Acerca de...Deposita en RODINPolíticasNormativasDerechos de autorEnlaces de interésEstadísticasNovedadesPreguntas frecuentes

RODIN está accesible a través de

OpenAIREOAIsterRecolectaHispanaEuropeanaBaseDARTOATDGoogle Académico

Enlaces de interés

Sherpa/RomeoDulcineaROAROpenDOARCreative CommonsORCID

RODIN está gestionado por el Área de Biblioteca, Archivo y Publicaciones de la Universidad de Cádiz

ContactoSugerenciasAtención al Usuario