High-Quality SiO2/O-Terminated Diamond Interface: Band-Gap, Band-Offset and Interfacial Chemistry

Thumbnail
Identificadores

URI: http://hdl.handle.net/10498/29544

DOI: 10.3390/NANO12234125

ISSN: 2079-4991

Ficheros
2022_979.pdf (2.433Mb)
Estadísticas
Ver estadísticas
Métricas y Citas
 
Compartir
Exportar a
Exportar a MendeleyRefworksEndNoteBibTexRIS
Metadatos
Mostrar el registro completo del ítem
Autor/es
Cañas Fernández, Jesús; Fernández de los Reyes, DanielAutoridad UCA; Zakhtser, Alter; Dussarrat, Christian; Teramoto, Takashi; Gutiérrez Peinado, MarinaAutoridad UCA; Gheeraert, Etienne
Fecha
2022-12
Departamento/s
Ciencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánica
Fuente
Nanomaterials, Vol. 12, Núm. 23, 2022
Resumen
Silicon oxide atomic layer deposition synthesis development over the last few years has open the route to its use as a dielectric within diamond electronics. Its great band-gap makes it a promising material for the fabrication of diamond-metal-oxide field effects transistor gates. Having a sufficiently high barrier both for holes and electrons is mandatory to work in accumulation and inversion regimes without leakage currents, and no other oxide can fulfil this requisite due to the wide diamond band-gap. In this work, the heterojunction of atomic-layer-deposited silicon oxide and (100)-oriented p-type oxygen-terminated diamond is studied using scanning transmission electron microscopy in its energy loss spectroscopy mode and X-ray photoelectron spectroscopy. The amorphous phase of silicon oxide was successfully synthesized with a homogeneous band-gap of 9.4 eV. The interface between the oxide and diamond consisted mainly of single- and double-carbon-oxygen bonds with a low density of interface states and a straddling band setting with a 2.0 eV valence band-offset and 1.9 eV conduction band-offset.
Materias
silicon oxide; diamond; interface; band-gap; band-offset; EELS; XPS
Colecciones
  • Artículos Científicos [12009]
Atribución 4.0 Internacional
Esta obra está bajo una Licencia Creative Commons Atribución 4.0 Internacional

Listar

Todo RODINComunidades y ColeccionesPor fecha de publicaciónAutoresTítulosMateriasEsta colecciónPor fecha de publicaciónAutoresTítulosMaterias

Mi cuenta

AccederRegistro

Estadísticas

Ver Estadísticas de uso

Información adicional

Acerca de...Deposita en RODINPolíticasNormativasDerechos de autorEnlaces de interésEstadísticasNovedadesPreguntas frecuentes

RODIN está accesible a través de

OpenAIREOAIsterRecolectaHispanaEuropeanaBaseDARTOATDGoogle Académico

Enlaces de interés

Sherpa/RomeoDulcineaROAROpenDOARCreative CommonsORCID

RODIN está gestionado por el Área de Biblioteca, Archivo y Publicaciones de la Universidad de Cádiz

ContactoSugerenciasAtención al Usuario