Stratigraphy of a diamond epitaxial three-dimensional overgrowth using doping superlattices

Identificadores

URI: http://hdl.handle.net/10498/30524

DOI: 10.1063/1.4948373

ISSN: 0003-6951

Ficheros
Acceso cerrado (1.041Mb)
Estadísticas
Ver estadísticas
Métricas y Citas
 
Compartir
Exportar a
Exportar a MendeleyRefworksEndNoteBibTexRIS
Metadatos
Mostrar el registro completo del ítem
Autor/es
Lloret Vieira, Fernando ManuelAutoridad UCA; Fiori, Alexandre; Araújo Gay, DanielAutoridad UCA; Eon, David; Villar Castro, María del PilarAutoridad UCA; Bustarret, Etienne
Fecha
2016
Departamento/s
Física Aplicada
Fuente
Applied Physics Letters, Vol. 108, Núm. 18
Resumen
The selective doped overgrowth of 3D mesa patterns and trenches has become an essential fabrication step of advanced monolithic diamond-based power devices. The methodology here proposed combines the overgrowth of plasma-etched cylindrical mesa structures with the sequential growth of doping superlattices. The latter involve thin heavily boron doped epilayers separating thicker undoped epilayers in a periodic fashion. Besides the classical shape analysis under the scanning electron microscope relying on the appearance of facets corresponding to the main crystallographic directions and their evolution toward slow growing facets, the doping superlattices were used as markers in oriented cross-sectional lamellas prepared by focused ion beam and observed by transmission electron microscopy. This stratigraphic approach is shown here to be applicable to overgrown structures where faceting was not detectable. Intermediate growth directions were detected at different times of the growth process and the periodicity of the superlattice allowed to calculate the growth rates and parameters, providing an original insight into the planarization mechanism. Different configurations of the growth front were obtained for different sample orientations, illustrating the anisotropy of the 3D growth. Dislocations were also observed along the lateral growth fronts with two types of Burger vector: b 01 1 = 1 2 [01 1 ] and b 112 = 1 6 [112]. Moreover, the clustering of these extended defects in specific regions of the overgrowth prompted a proposal of two different dislocation generation mechanisms.
Colecciones
  • Artículos Científicos [12014]
  • Articulos Científicos CC. Mat. [579]
  • Articulos Científicos Fis. Ap. [317]

Listar

Todo RODINComunidades y ColeccionesPor fecha de publicaciónAutoresTítulosMateriasEsta colecciónPor fecha de publicaciónAutoresTítulosMaterias

Mi cuenta

AccederRegistro

Estadísticas

Ver Estadísticas de uso

Información adicional

Acerca de...Deposita en RODINPolíticasNormativasDerechos de autorEnlaces de interésEstadísticasNovedadesPreguntas frecuentes

RODIN está accesible a través de

OpenAIREOAIsterRecolectaHispanaEuropeanaBaseDARTOATDGoogle Académico

Enlaces de interés

Sherpa/RomeoDulcineaROAROpenDOARCreative CommonsORCID

RODIN está gestionado por el Área de Biblioteca, Archivo y Publicaciones de la Universidad de Cádiz

ContactoSugerenciasAtención al Usuario