Atomic composition of WC/ and Zr/O-terminated diamond Schottky interfaces close to ideality
Identificadores
URI: http://hdl.handle.net/10498/30203
DOI: 10.1016/j.apsusc.2016.04.166
ISSN: 0169-4332
Ficheros
Estadísticas
Métricas y Citas
Metadatos
Mostrar el registro completo del ítemFecha
2016-04-27Departamento/s
Ciencia de los Materiales e Ingeniería Metalúrgica y Química Inorgánica; DidácticaFuente
Applied Surface Science 395 (2017) 200–207Resumen
Electrical and nano-structural properties of Zr and WC-based Schottky power diodes are compared andused for investigating oxide-related effects at the diamond/metal interface. Differences in Schottky bar-rier heights and ideality factors of both structures are shown to be related with the modification of theoxygen-terminated diamond/metal interface configuration. Oxide formation, oxide thickness variationsand interfacial oxygen redistribution, associated with thermal treatment are demonstrated. Ideality fac-tors close to ideality (nWC= 1.02 and nZr= 1.16) are obtained after thermal treatment and are shown to berelated with the relative oxygen content at the surface (OCRWC= 3.03 and OCRZr= 1.5). Indeed, thermaltreatment at higher temperatures is shown to promote an escape of oxygen for the case of the WC diode,while it generates a sharper accumulation of oxygen at the metal/diamond interface for the case of Zrdiode. Therefore, the metal-oxygen affinity is shown to be a key parameter to improve diamond-basedSchottky diodes.
Materias
Diamond; Schottky; Oxygen-terminated; TEM; Power devicesColecciones