Metal–oxide–diamond interface investigation by TEM: Toward MOS and Schottky power device behavior

Estadísticas
Métricas y Citas
Metadatos
Mostrar el registro completo del ítemFecha
2014-06-23Departamento/s
Ciencia de los Materiales e Ingeniería Metalúrgica y Química InorgánicaFuente
Physica Status Solidi (A) Applications and Materials Science 2014 - Vol.211(10), pp. 2367-2371Resumen
Metal and oxide distribution in diamond metal–oxide–
semiconductor (MOS) structures are characterized using
several transmission electron microscopy (TEM) modes at
nanometric scale. To understand their electrical behavior,
oxygen distribution using electron energy loss spectroscopy
(EELS) through the layer structure, high-resolution electron
microscopy (HREM), and annular dark field (ADF) observations
are reported. Oxide thickness variations, as well as oxygen
content variations have been identified and characterized at an
atomic resolution. The latter allows to understand the related
electrical behavior as, for example, leakages or shortcuts.
Materias
diamond; oxide characterization; power device; schottky; TEMColecciones
- Artículos Científicos [12077]
- Articulos Científicos CC. Mat. [585]
- Artículos Científicos IMEYMAT [581]